gavinlg
Veteran
Just very quickly - the emulsion (under side) of my just developed 400tx negative is sticky after drying. It's like it has a very very thin sticky rubber coat....
Does anyone know what this means?
I fixed for 4 minutes, used d76 @ 9 3/4 mins and washed for about 10 minutes with photoflo as the last one, and then hung up to dry.
Does anyone know what this means?
I fixed for 4 minutes, used d76 @ 9 3/4 mins and washed for about 10 minutes with photoflo as the last one, and then hung up to dry.
Wimpler
Established
It means it isnt dry yet. Let it dry longer.
gavinlg
Veteran
Wimpler said:It means it isnt dry yet. Let it dry longer.
Thanks
I knew it was something simple... only other thing I could think of was the photo-flo I used (for the first time) Used 1/200 like it said and did it after washing for 30secs.
I'll let it dry out some more and see how it gets
Share: