gavinlg
Veteran
Just very quickly - the emulsion (under side) of my just developed 400tx negative is sticky after drying. It's like it has a very very thin sticky rubber coat....
Does anyone know what this means?
I fixed for 4 minutes, used d76 @ 9 3/4 mins and washed for about 10 minutes with photoflo as the last one, and then hung up to dry.
Does anyone know what this means?
I fixed for 4 minutes, used d76 @ 9 3/4 mins and washed for about 10 minutes with photoflo as the last one, and then hung up to dry.