andre mueller
Member
I'm sure some of you have done this already and can help me out.
I want to push 120 Trix in HC110 - dilB by increasing temperature instead of time.
I would use this graph from:
http://www.covingtoninnovations.com/hc110/
My questions is if I have to increase the frequency of agitation?
Does the developer exhaust itself faster at a higher temperature?
So far I do 2-3 inversions every minute after the initial agitation.
Would it matter at dilution B?
Would it change the look of the negative compared to pushing by increasing developing time?
This is what I developed today by pushing and overexposing 1 stop.
I quite like the tones.

I want to push 120 Trix in HC110 - dilB by increasing temperature instead of time.
I would use this graph from:
http://www.covingtoninnovations.com/hc110/
My questions is if I have to increase the frequency of agitation?
Does the developer exhaust itself faster at a higher temperature?
So far I do 2-3 inversions every minute after the initial agitation.
Would it matter at dilution B?
Would it change the look of the negative compared to pushing by increasing developing time?
This is what I developed today by pushing and overexposing 1 stop.
I quite like the tones.