Occasionally I've been getting some small sticky spots on the last few negs of each roll after they've been drying (by hanging in the shower recess). Is this residue from photoflo?
I've been developing 2 rolls at a time in a Patterson tank, and my routine is to rinse using the ilford method of three changes of water with 5, 10, 20 inversions. I let the water sit in the tank for a few minutes between changes. Lastly I do another change of water with photoflo and do maybe 10 inversions and drain. I use a small amount of photoflo. I shake the photoflo bottle and add the bubbly residue of the photoflo lid to the 600ml of water for that final rinse.
Any ideas?
I've been developing 2 rolls at a time in a Patterson tank, and my routine is to rinse using the ilford method of three changes of water with 5, 10, 20 inversions. I let the water sit in the tank for a few minutes between changes. Lastly I do another change of water with photoflo and do maybe 10 inversions and drain. I use a small amount of photoflo. I shake the photoflo bottle and add the bubbly residue of the photoflo lid to the 600ml of water for that final rinse.
Any ideas?