I've scoured the forums but could not locate this information. I am going for a high-contrast, low tonal range and large grain look for an upcoming series, so I ask:
What times and dilutions are you using to push Tri-X 400 to 1600 and 3200 with Dektol 1:3 or 1:10?
I have a jug of Dektol premixed at 1:3, but I can easily reduce the concentration to 1:10 by adding two parts water in the development tank.
In addition, has anyone used Dektol with Neopan Acros 100; 400 or Fomapan 100? What times / dilutions? Have you successfully been able to push these films as well?