atlcruiser
Part Yeti
I am tired of inverting tnks and I go through too many roll of film; my elbow is sore!
I picked up a roller base in the RFF classifieds. Mostly I use patterson tanks but I also have JOBO. Looks to me like most tanks will fit just fine and the base has an auto revese direction.
The tanks are marked and it is on the web the volume of chemicals to use with hand and roller so I have that. All of my c-41 and e 6 chemistry gives detailed info on using a roller system.
I am a bit in the dark on B+W. I generally use rodinal 1:50 or d 76 1+1. The rodinal times are based on ASA and vary from 16min to 60. Normally I invert for the frst 30 seconds then 3 nversions per 30' , per min or per 3 min depending n the overall development time required. D 76 1+1 is mor eor less the same basic system How best do I translate this to roller time?
thanks
I picked up a roller base in the RFF classifieds. Mostly I use patterson tanks but I also have JOBO. Looks to me like most tanks will fit just fine and the base has an auto revese direction.
The tanks are marked and it is on the web the volume of chemicals to use with hand and roller so I have that. All of my c-41 and e 6 chemistry gives detailed info on using a roller system.
I am a bit in the dark on B+W. I generally use rodinal 1:50 or d 76 1+1. The rodinal times are based on ASA and vary from 16min to 60. Normally I invert for the frst 30 seconds then 3 nversions per 30' , per min or per 3 min depending n the overall development time required. D 76 1+1 is mor eor less the same basic system How best do I translate this to roller time?
thanks