Question for folks who have used 4x5 TMAX 400 and HP5+. Do you feel that TMAX is worth the extra .60 cents or so per sheet? What do you feel are the benefits of using TMAX 400 vs HP5+
I'd be looking to develop the TMAX 400 in TMAX developer at 1-9 for 20 minutes at 68 degrees (Massive Development Chart) vs Kodak's recommended 1-4 for 8.5 minutes at 68 degrees. Has anyone used the 1-9 ration rather then the standard 1-4?
My reason for going with 1-9 vs 1-4 it isn't to save money but rather the fact that it takes about 30 second to fill my Yankee 4x5 tank and I'm not sure that 8.5 minutes is enough time for proper even development.
Note would likely do a few test sheet with both to see which works best.
Thanks Mike
I'd be looking to develop the TMAX 400 in TMAX developer at 1-9 for 20 minutes at 68 degrees (Massive Development Chart) vs Kodak's recommended 1-4 for 8.5 minutes at 68 degrees. Has anyone used the 1-9 ration rather then the standard 1-4?
My reason for going with 1-9 vs 1-4 it isn't to save money but rather the fact that it takes about 30 second to fill my Yankee 4x5 tank and I'm not sure that 8.5 minutes is enough time for proper even development.